Pretreatment method of plating: electrochemical deoiling method (i.e. electrolytic deoiling method)
Purpose of cleaning: to remove oil
Process formula: the oiled parts are taken as an electrode (commonly used cathode) and DC voltage is added, the electrolyte is 10-20% NaOH or soda soda, and the working temperature is 30-80℃